Links:

Melting Points of Polymers

Polymer Name Tm1
(K)
Poly(tetramethylene oxide), PTMO 314, 333
Poly(ethylene adipate) 336
Poly(ethylene oxide), PEG 339
Poly(trans-1,4-butadiene) 371
PoIy(1-butene), isotactic 398
Poly(ethylene) 414
Poly(methyl methacrylate), isotactic 417
Poly(trans-1,4-butadiene) 417
Poly(methylene oxide), POM 445
Poly(vinylidene fluoride) 450
Poly(propylene), isotactic 452
Poly(ω-undecanamide), Nylon 11 460
Poly(vinylidene chloride) 468
Poly(vinyl fluoride) 472
Poly(methyl methacrylate), syndiotactic 473
Poly(decamethylene sebacamide), Nylon 10,10 475
Poly(vinyl chloride) 493
Poly(caprolactam) 495
Poly(6-aminocaproic acid) 497
Poly(hexamethylene sebacamide), Nylon 6,10 497
Poly(vinyl alcohol) 504
Poly(decamethylene adipamide), Nylon 10,6 508
Poly(hexamethylene suberamide), Nylon 6,8 509
Poly(styrene), isotactic 515
Poly(4-methylpentene) 516
Poly(ethylene terephthalate), PET 537
Poly(hexamethylene adipamide), Nylon 6,6 545
Poly(styrene), syndiotactic 549
Poly(vinyl chloride), PVC 578
Poly(acrylonitrile), syndiotactic 594
Poly(etheretherketone) 630
Poly(para-xylylene) 697
1The Tms are the average of several experimental values.